I use stone of gabro diabaz 3-20mm and sand 0.1-1.2. 6 types of dimensions at all. Vibrate very strong 2-3 hour. Epoxy CR80 350mPas if it have diluent and will be shrinkage .. it very bad for as....
Type: Posts; User: Obivan
I use stone of gabro diabaz 3-20mm and sand 0.1-1.2. 6 types of dimensions at all. Vibrate very strong 2-3 hour. Epoxy CR80 350mPas if it have diluent and will be shrinkage .. it very bad for as....
Finally we make first bed 250kg 1000x600x300mm. I think bubbles not so much. Mixture 9% of weight of aggreate. Next time i'm ready to reduce to 8-8.5%. What time to dry out so big bed frame for...
The producer Biresin CR80 sika does not reveal the secret about included or not difunctional reactive dilluent. Only i know about it : bisphenol-A-(epichlorhydrin) and epoxy resin (number average...
So i looking for true epoxy in my counry (Russia). Only Sika Biresin CR80 and Biresin LS is available. CR83 and Gurit Prime 27 its not available. May be something else good epoxy?
hi peter and all.
What is resin 100% solid for infusion? What are they based on ? why do they have low viscosity
What resin uses in industrial commercial mixing like Rampf , Schneeberger, Studer?...
Is anybody try to use low viscosity epoxy like DOW DER3271 or Hexion Epikote 05102 bisphenol A and with difunctional reactive dilluent. The viscosity about 200-400mPas. Mixture with 8% by weight it...