Hi Thomas - One of their mixes claims E=80GPa. Give that a go. I expect in flexure it will be lower than the compression value. That would be interesting. I tried to get some shipped here some years ago but they would not sell it outside EU. Some of the gouts and cretes I see here now have the compression modulus and the acoustic or "dynamic" modulus quoted. The acoustic modulus is usually close to the compression modulus. Unfortunately, the acoustic is a compression process so they are similar. Need a pure tension test to really see the delta. Peter
larger aggregate is cheaper less processing and fills large gaps.